Gravity Die Casting vs High Pressure: The Decision That Determines Whether Your Part Can Be Heat Treated
Meta description: When to choose gravity permanent mould casting over High Pressure Die Casting for aluminium parts — T6 compatibility, porosity differences, wall thickness minimums, tool life trade-offs, and the batch volume thresholds where each process makes financial sense.

gravity die casting and high pressure die casting aluminium casting services comparison

The question usually arrives partway through a design review, after the decision has effectively already been made. The drawing says "aluminium die casting, T6 condition." The project engineer assumed die casting meant high pressure die casting. The foundry engineer is now explaining, politely, that T6 and high pressure die casting are a combination that reliably produces blistered parts.

💡 Key Insight: It happens enough that it's worth setting out the two processes clearly — not as an academic comparison, but as a practical routing decision with real cost and schedule consequences.

What gravity die casting actually is
Gravity permanent mould casting uses a steel die, like high pressure die casting. The difference is how metal enters the cavity. In high pressure die casting, molten aluminium is driven in at 600–1,000 bar through a shot sleeve and plunger, filling the cavity in a fraction of a second. In gravity casting, metal is poured or slowly tilted into the cavity under — as the name suggests — gravity alone, with no applied pressure.

high pressure versus gravity permanent mould aluminium casting comparison

The table captures the main parameters. The one that drives most routing decisions is the T6 row. High pressure die casting entraps gas — air and lubricant vapour from the shot sleeve — in the casting. The porosity that results is not visible on the surface and usually doesn't fail dimensional inspection. But when you put the part through T6 solution treatment at 490–530°C, those trapped gas pores expand. The surface blisters. The part is scrap.

When this actually matters
T6 becomes relevant when the application needs elongation above about 3–4% — when the part must deform rather than crack in an impact or overload scenario. Structural nodes, safety-critical brackets, and load-bearing housings in aerospace and automotive powertrain are the common cases.

The cost and volume equation
Gravity casting tooling costs less than high pressure die casting tooling. A steel permanent mould for a medium-complexity part typically runs 30–60% of the equivalent high pressure die. The trade-off is cycle time. A gravity casting cycle — pour, dwell, open, extract, coat — runs 60–120 seconds per part. A high pressure die casting cycle on a comparable part runs 20–40 seconds.

T6 heat treatment of aluminium casting parts

The heat treatment process itself
T6 heat treatment for aluminium gravity castings is a three-stage operation: Solution treatment, Quench, and Artificial ageing. The furnace uniformity requirement is AMS 2750 or equivalent — temperature variation across the working zone must be held within ±5°C at temperature.

Get a Quote

FAQs

Can high pressure die casting parts be T6 heat treated? Standard high pressure die castings are not recommended for T6 due to subsurface gas porosity.
What alloy is used for gravity die casting? A356 and its variants (A356.2, A357) are the standard alloys for structural gravity permanent mould castings.
What is the minimum batch size for gravity die casting? The process is economically viable from roughly 200 parts per year upward.